QAR: Click Here
Conditions for approval required by: Julien Gauther

Certification of Aerospace Products to international quality Standards
Form restricted to registered, logged in users. Please return to the home page and use the Create Account option.
In test report, “Dureté / hardness” section: HV5 9999 is written. This is just, to me, a typo and hopefully, hardness test results (HRC units) are listed in “Metallurgie” section. Thus, this is not blocking, just something to point out.
Actual sample size for hardness test is in line with EN3004, table 6, column B (destructive test). For acceptance, EN3004 specifies hardness test sample size as per table 6, column A (non-destructive tests). However, hardness test is seen as a destructive test. Thus, agreed, just something to mention.
To conclude, some some comments that are not blocking.
Best regards
Julien